Plating silver on steel




Does anyone know if silver can be plated to stainless steel?

Tino Volpe
- Cumberland, Rhode Island
2006


One way is to Woods nickel strike, silver strike and silver plate.

James Watts
- Navarre, Florida
2006


Answer is yes but first you must activate stainless steel. Hope it helps and good luck!

Goran Budija
- Cerovski vrh Croatia
2006




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2025 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"