Aluminide Coating Stripper




We are looking for an Environmentally friendly stripper for Alumide coating. Currently using ASC 2-N (bifluoride + Nitric)
Thanking you in advance

Sridhar Bushigampala
Orenda Aerospace - Ontario, Canada
2006
publicly reply to Sridhar Bushigampala

We use the same. If you are having a tough time due to the parts being in high temperature environment, use straight 25% nitric at 70-100 degree F for thirty minutes. We accomplished this after a normal stripping cycle. Heat tint results were excellent.

Dan Gac
- Phoenix, Arizona, USA
December 15, 2011
publicly reply to Dan Gac



(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2025 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"