Marine paints




Dear sir
we have some small panels that are used in electronic equipment.
these electronic equipments are used in ships.
does anyone knows how many hours of salt spray these panels resist if marine paints applied on them?
regards

Joe Fisherman
Aftab Company - Ankara, Turkey
2006



2006

Salt spray testing is an accelerated corrosion test that has little to do with real life use. It is at best an indicator.
That said, painting is like plating, how well it performs is quite dependent on who applied it.
So, the only way to answer your question is to coat it and do salt spray testing.

James Watts
- Navarre, Florida




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2025 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"