ted_yosem
Curated with aloha by
Ted Mooney, P.E. RET
finishing.com -- The Home Page of the Finishing Industry

  The authoritative public forum
  for Metal Finishing 1989-2025
  mfhotline


  -----

How to peeloff the wrong color Powder Coated?




Dear sir,

To one of our customer, we have wrongly coated with Deep Orange instead of Ivory White.
As I had coated with ivary white over the deep orange there is a mixing of color.
For that matter I need to peel off the old color ( Deep Orange ) & powder coat with Ivory
White. Please suggest me in this regard as early as possible as our customer is waiting for despatch.

with regards,

S R Ithal
Parallel Track - Bangalore, Karnataka, India
2006


Please use paint stripper and remove wrongly powder coated color.

S.Palanismy
- Hosur, T.N., India
2007




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2025 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"