RoHS and zinc plated hardware



Are you saying (ref. letter 36234) that Zinc Plated washers and retaining rings are compliant? I thought my vendor said they were not.

Susan Hotkowski
- Old Saybrook, Connecticut, USA
2006



First of two simultaneous responses --

It's not the Zinc but the chromate that is at issue.
It is the chromate. Hexavalent chromates on zinc or aluminum would not be considered RoHS compliant.

Bill Grayson
metal finishing - San Jose, California, USA
2006



Second of two simultaneous responses --

Zinc plated anything which has a trivalent conversion coating or non chrome coating is generally compliant. Ask your vendor to certify that parts are RoHS compliant.

Gene Packman
process supplier - Great Neck, New York
2006




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2025 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"