How to convert the color of GALVANIZED IRON to SILVER?




I WOULD LIKE TO KNOW HOW TO CONVERT THE COLOR OF GALVANIZED IRON INTO SILVER, BUT I don't KNOW THE PROCESS... IS THAT POSSIBLE?...

Gonzalvo Ruizo Jr.

2006


There are silver color paints with or without lacquer topcoats. Also possible is to strip the zinc (galvanize) and silver plate.

Guillermo Marrufo

2006


There are SPECIAL ZINC ALLOY available from Australia etc or You can make it yourself by mixing antimony, tin, aluminium and lead to form a alloy. Use this alloy in little preparation in the Zinc bath.

S.K.Subramanian

2006




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2025 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"