Metal finishers helping each other -- No cost, No registration, No damn popups
(we earn from 'affiliate link' purchases, making the site possible)

Home /
T.O.C.
Fun
FAQs
Good
Books
Ref.
Libr.
Adver-
tise
Help
Wanted
Current
Q&A's
Site 🔍
Search
ted_yosem
Curated with aloha by
Ted Mooney, P.E. RET
finishing.com -- The Home Page of the Finishing Industry

  The authoritative public forum
  for Metal Finishing 1989-2025
  mfhotline


  -----

Knowledge of D M Plant



Dear Sir,

I am working in perfume company and I want to know about D M Water, How to make it and what is the required for that.

Ashwin Rajput

2006



Hi,
D.M water means Demineralised water. Water generally contains anions and cations(read basic chemistry) and the specially made resins available from ION Exchange limited and so many other suppliers can be used to remove these ions from water and the final out put is D.M Water. Try to contact water treatment suppliers.

S.K.Subramanian

2006




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2025 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"