How to improve finish on titanium balls





I am having a problem getting a mirror finnish on some titanium balls. Do you have any suggestions on how I can achieve this finish!

SHAWN K WYBLE
BALL GRINDING AND FINISHING - OAK HARBOR, Ohio
2005



First of two simultaneous responses --

How about switching to electropolishing titanium in house? We can provide safe electrolyte and instructions.

anna_berkovich
Anna Berkovich
Russamer Lab
supporting advertiser
Pittsburgh, Pennsylvania
russamer labs banner
2005



Second of two simultaneous responses --

Suggest a mass finishing system. What media you use depends on your volume and/or how fast you want your process. Meaning you can do either a wet or dry process.

tony kenton
AF Kenton
retired business owner - Hatboro, Pennsylvania
2005




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2025 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"