Electro galvanized finish for anchor bolts





Currently, I am working in steel building manufacturing company. I want to know disadvantages and advantages, instead of hot-dip galvanizing finish if electro galvanized finish is given to J-type steel anchor bolt which needs to be embedded in the concrete. What will be its behavior and result?

Mehaboob
steel - Saudi Arabia
2005



"Handbook of Hot Dip Galvanization"
by Maass & Peissker
galv_hot_dip_handbook2011
on AbeBooks

or eBay or

Amazon

(affil links)

Mehaboob: Hot dip galvanizing will provide long-term corrosion protection on the J-bar anchors. The coating must be thin enough to accept the nuts which will go on the parts after going into the cement.

Daryl Spindler
Daryl Spindler, CEF
decorative nickel-chrome plating - Greenbrier, Tennessee
2005




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2025 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"