Is Dacro coating RoHS compliant?





We supplied zinc plated leveler to the US customer and it failed to be RoHS compliant. Now we want to change using Dacro coating but not sure is it RoHS compliant or not?

Your help would be appreciated!

Richard Huang
caster factory - Guangzhou, Guangdong, China
2005



2005

Sounds like that US customer has saved a bundle so far :-)

"Dacro" is a trade name, Richard, so it contains what the vendor decides it contains on a given day. But my understanding is that the vendor labels the RoHS complaint version Geomet rather than Dacromet. Good luck!

Ted Mooney, finishing.com
Ted Mooney, P.E.
Striving to live Aloha
finishing.com - Pine Beach, New Jersey



Geomet is definitely RoHS compliant and a product of Dacral Coating Ltd

Regards

Balaji.C
- Chennai,Tamil Nadu and India
September 29, 2008




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2025 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"