Enamel steel test




I want to ask about if there is any speed test can be applyied on steel to detect if it will be cause a problem after enamel painting?

Mohamed Mahmoud Hanafy
enamel business - Cairo, Egypt
2005



2005

Dear Mohamed Mahmoud Hanafy
You ask about if there is any tests for steel before painting it by enamel.
Yes as you know there are special steel alloys suitable for enamel painting and those steel must be have aspical chemical composition and physical proparties and you must make analysis for steel and compaire it with eur standard EN 10209.
There is a very important test for steel before paint it is fish scales test and you can do it by special enamel formula to test the quality of steel.

Aly Gomaa
- Cairo, Egypt




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2025 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"