ted_yosem
Curated with aloha by
Ted Mooney, P.E. RET
finishing.com -- The Home Page of the Finishing Industry

  The authoritative public forum
  for Metal Finishing 1989-2025
  mfhotline


  -----

Low stress electroless nickel + immersion gold




Which specialist investigates about low stress electroless nickel + immersion gold process for PCB manufacturing industry?
how it effects Flex board bending OR other performance?
who can tell me more information about them?
thanks for your attention.

Ge FX
Ts - SH, CN
2005



If your question is where to find a consultant to retain for this, Ge, our Directory of Consultants is a good place to start. If you are asking to start a public dialog on the subject, results are always better when you start the dialog by introducing yourself, your own problem, and your progress to date. Good luck.

Ted Mooney, finishing.com
Ted Mooney, P.E.
Striving to live Aloha
finishing.com - Pine Beach, New Jersey
2005



2005

Ge FX,
Your suppliers might help you in determining the stress in electroless nickel.
Usually they are semi bright electroless Nickels.
We are successfully plating Immersion Gold on electroless nickel for Flex boards with out any problems for years now.

Sridhar Bushigampala
- Toronto, ON, Canada




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2025 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"