Best metal for your electrodes?





Ok. I am making wet cell batteries filled with lemon/lime/grapefruit juice for my 8th grade science fair project and I need to know what would be the best metals to use for the elecrodes. I was thinking maybe copper anodes and zinc cathodes. is that good enough or can I go with a better combination?
any advice would be very much appreciated.

Johnny C [last name deleted for privacy by Editor]
student - Redding, California, USA
2005



Good choice, Johnny!

Ted Mooney, finishing.com
Ted Mooney, P.E.
Striving to live Aloha
finishing.com - Pine Beach, New Jersey
2005



Excellent choice - you won't do much better than that.

trevor crichton
Trevor Crichton
R&D practical scientist
Chesham, Bucks, UK
2005


adv.: Supplier of Copper Anodes, Nickel Anodes, Bismuth Metal, & Other Metal Products for Industry & The Arts
carter banner



(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2025 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"