RUSTING OF IORN BARS INSIDE CONCRETE DUE TO RAIN WATER SEEPAGE





Dear sir
can you pl advice me on how to prevent rusting of steel bars inside concrete cealing due to rain water seepage. Can I use a water based rust converter this on eBay or Amazon [affil links] and allow the puddle to be stagnant over the leak area so that the converter can seep through and perform.
Pl advice.
Thanks and regards,

A M WILSON
personal issue - CHENNAI, INDIA
2005


The only answer I know of to this problem is the coating of the rebar with epoxy resin coatings before laying in the concrete. After the fact, rip out and redo.

Gene Packman
- Great Neck, New York
2005




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2025 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"