  Thread 371/09

Mirror finish of stainless steel wire product




We make stainless steel wire products and want to have mirror finish of the same... what process we should adopt?

Nayeem ahmed
MKB India,Inc - Delhi, India
2005
publicly reply to Nayeem ahmed


You would need to mechanically polish the items you manufacturer, and/or electropolish them. It's hard to say how much of this should be done while it's still wire vs. how much should be done on finished parts, and whether electropolishing is beneficial, without looking at an exact product and its application.

Ted Mooney, finishing.com
Ted Mooney, P.E.
Striving to live Aloha
finishing.com - Pine Beach, New Jersey
2005
publicly reply to Ted Mooney

Dear Ted, Thanks for your response. We will get back to you with product and its application.

Nayeem
MKB India,Inc. - Delhi, India
2005
publicly reply to Nayeem



(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2025 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"