Recovering used IPA (Isopropyl Alcohol)




I am the Pollution Control Officer of an Electroplating Company here in the Philippines. Our company used Isopropryl alcohol for washing some materials. Because of this, we are generating Used IPA. I would like to know other means of reusing said Used IPA or its means of recovery or disposal.

Thank you...

Reina P. YAp
Electroplating - Philippines
2005


Try Distilling the IPA and see if its of sufficient puriety for re-use.

Peter Van de Luecht
- Melbourne, Vic, Australia
2005


In the USA there are several companies that sell small stills for recovering solvents. The IPA will be fairly pure, but not as good as new material.

James Watts
- Navarre, Florida
2005



Our group is using IPA for cleaning. Our problem is how to disposed used IPA?

Is there a company in the Philippines that handles IPA disposal (within Metro Manila or neighboring provinces)?

R Vinoya
- Philippines
July 6, 2011




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2025 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"