Gold plating details




Sir,

I'm doing my Graduate degree in the decipline of chemical engineering.
As I'm final year student I'm in position to submit the Projectwork to my college.
My profeesors given the topic of "Gold plating of brass ornaments".I have tried in several websites and industries regarding the electrolyte composition,pretreatment. But I am not getting any support.please help me & guide me to complete the project.

Jaganathan.M
Student - Salem, Tamilnadu, India
2005



Hello Jaganathan. Have you gotten this far in your education without using textbooks? I can't imagine learning thermodynamics and heat transfer and other chemical engineering disciplines by browsing websites. The point being that to efficiently learn what you need to learn about gold plating, you need textbooks not websites. Please see our "must have" booklist. Good luck.

Ted Mooney, finishing.com
Ted Mooney, P.E.
Striving to live Aloha
finishing.com - Pine Beach, New Jersey
2005




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2025 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"