Metal finishers helping each other -- No cost, No registration, No damn popups
(we earn from 'affiliate link' purchases, making the site possible)

Home /
T.O.C.
Fun
FAQs
Good
Books
Ref.
Libr.
Adver-
tise
Help
Wanted
Current
Q&A's
Site 🔍
Search
ted_yosem
Curated with aloha by
Ted Mooney, P.E. RET
finishing.com -- The Home Page of the Finishing Industry

  The authoritative public forum
  for Metal Finishing 1989-2025
  mfhotline


  -----

Looking for unsharpened razor blade source



1999

Q. Looking for source for unsharpened razorblades for thickness testing purposes.

David M. Weaver [deceased]
- Toccoa, Georgia

Ed. note: With great sadness we must advise that David passed awayt on Aug. 15, 2003.


A. Palm Commodities out of Laverne, TN supplies unsharpened razor blades.

Megan Pellenz
Megan Pellenz
- Syracuse, New York
1999




Razor blades as plating thickness measurement coupons?

Q. What is your opinion on using razor blades for coupons to measure the plating on steel? The measurements are wack and the blade seems to be shrinking due to the chemical. This is in regards to the nickel plating process.

GUNTHER BUMPKIIN
- HARRISON. Arkansas
February 6, 2020




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2025 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"