Common phosphating for both CRC and aluminum components?




Is there any common spray phosphating which works on both crc and aluminum components?

Manish Dhyani
UL - New Delhi, India
2005



Yes, Manish. These "dual metal" phosphatizing solutions are readily available from most of the suppliers of pretreatment chemicals. Phosphatizing is not the ultimate pretreatment for aluminum, but it's serviceable.

Ted Mooney, finishing.com
Ted Mooney, P.E.
Striving to live Aloha
finishing.com - Pine Beach, New Jersey
2005



Dear Manish Dhyani,

You can use a common treatment solution for phosphating of steel and aluminium components. These baths usually have fluoride salts as one of the constituents, to complex the aluminium.

T.S.N. Sankara Narayanan
T.S.N. Sankara Narayanan
- Chennai, Tamilnadu, India
(ed.note: The good doctor offers a fascinating blog, "Advancement in Science" )
2005



Dear Sankara Narayanan
I study effecrs of fluoride ion (F-)in phosphating
please give me advice about it's reference.
best regards,

Mohamad Mahdiz
ms student - Tehran, Iran
2007




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2025 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"