Protection for Patina Finishes on Brass Watch Dials



We are one of the leading manufactures of watch dials and hands in India. We are carrying out various types of electroplating processes and also some patina finishes on brass. In patina finish we are facing some problem that is we are not able to give protection for the finished surface as the colour discolours after some time. I would like to know any dip type water based clear lacquer is available for the process and also the manufacturer of water based dip lacquers. We need only dip type as our component watch hands very small in size.

Nandini Umesh
Kamla dials and devices Ltd. - Bangalore, Karnataka, India
2004



Water Based Lacquer

on Amazon

(affil links)

Do it yourself water based lacquer:

shellac(bleached or orange)..6 oz. borax this on eBay or Amazon [affil links] ..........1 1/2 oz.
water..........1 pt.
Boil together until lac is dissolved!

According to Scyentific American Cyclopaedia of Formulas, New York 1910. (www.thelitterbox.org/librum/i_sacof/669.gif)

Goran Budija
- Cerovski vrh Croatia
2004




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2025 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"