I need Epoxys for Operating Temp of -40f to +150f





2004

I am assembling a product for the Oil & Gas industry and I need to glue a Aluminum Circular Connector into an Aluminum Tube approx. 1" in dia. This product needs to operate at -40f to 150f. What expoxy is recommended to work within these temps? The volumes will be large so I need data before I specify the correct epoxy manufacture.

I have looked at the 3M web site but can not find data on these operating temps.

Regards,

RICK HAWRYLAK
SIGMA MARKETING & SALES INC. - KATY, Texas

Try MasterBond.com. I seem to recall an ad for an adhesive good from liquid Helium temperature thru 300 or 400 F.

Tom Gallant
- Long Beach, California, USA
2004




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2025 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"