  Thread 323/73

Materials that can be coated with Teflon?




Greetings !

I wonder if it is application of Teflon coating or any other non-stick coating limited to only metal or is possible to coat any other material !? Stone, marble, concrete,...?

Could someone describe coating process little bit more precisely?!

Can I do it on my own at home ?

With best regards!

Uros Ocepek
hobbyist - Novo mesto, Slovenia
2004
publicly reply to Uros Ocepek

Yes you can coat all tha surfaces that resist the curing themperature (about 380°C). There are also low bake temperature teflon coatings.

You can learns more about the teflon coating process at www.fisasa.com/teflon_proceso.htm

Best regards,

Jordi Pujol
- Barcelona, Spain
2004
publicly reply to Jordi Pujol



(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2025 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"