Zinc Flake/Chromate coating




Q. Has anyone heard of a Zinc Flake/Chromate coating per MIL-C-87115 [link is to free spec at Defense Logistics Agency, dla.mil]? I found the spec. but can't seem to find a manufacturer or anyone that is familiar with it.

jim conner
Jim Conner
Anoplex Software
supporting advertiser
Mabank, Texas USA
Anoplex logo


A. I'm not sure, Jim, but I think you are referring to the zinc-rich dip-spin coatings like Dacromet and Magni.

Ted Mooney, finishing.com
Ted Mooney, P.E.
Striving to live Aloha
finishing.com - Pine Beach, New Jersey
1999


April 13, 2016

A. Zinc flake/chromate coatings under this mil spec refer to non-electrolytic processes usually referenced to trademarked coatings, which Magni has, but a number of other suppliers also provide.

Robert Ries
- Goshen, Indiana USA
1999




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2025 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"