Deburring material for pen clips





2004

DEAR SIR,

WE ARE MFG. OF PEN CLIPS. I WANT TO KNOW WHATS MATERIAL USING IN DEBURRING. NOW I AM USING EMERY this on eBay or Amazon [affil links] AND CAUSTIC .

Please ADVICE ME

THANKING YOU

Sushil Bohra
DEBURRING OF METAL CLIPS - MALAD (w), MUMBAI, MAHARASHTRA, INDIA



What is the material? Brass? If so, you might need a one or 2 step operation in a mass finishing system. Are parts going to be plated? Need to know before I can recommend properly.

tony kenton
AF Kenton
retired business owner - Hatboro, Pennsylvania
2004


I ASSUME YOU ARE referring TO HARDENED PEN CLIPS IF ITS CORRECT FIRST STEP SHOULD BE DESCALING AND SMOOTHING USING CERAMIC IN VIBRATORY MACHINE AND SECOND STEP POLISHING IN SAME MACHINE WITH PORCELAIN MEDIA AND POLISHING CHEMICAL TO GET PRE PLATE FINISH.

Prasad
- Mumbai, India
2004




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2025 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"