Coating to Protect an Aluminum Casting Against Hydrochloric Acid




We are looking for a coating to protect an aluminum casting in a hydrochloric acid environment. Any help with this situation would be greatly appreciated.

Jon Sieminski
Manufacturing - Gowanda, New York, USA
2004
publicly reply to Jon Sieminski

What was the answer to his letter.

John Cadden
- Canton, Ohio
2006
publicly reply to John Cadden


The question was too vague to have a clear-cut answer, but plastisol coating of the parts is one possibility. Good luck.

Ted Mooney, finishing.com
Ted Mooney, P.E.
Striving to live Aloha
finishing.com - Pine Beach, New Jersey
2006
publicly reply to Ted Mooney



(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2025 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"