Looking for copper roll to use as bar top




Q. remodel and build out pubs/bars. My owner has a copper fixation. I am looking for the copper to use as a bar top. (26" x 44') Can't find the real thing anywhere. Please direct me. Thanks a million

R. Bruce Watson
contractor - Atlanta, Georgia, USA
2004



Q. Is there a supplier of copper sheeting to be used on a countertop in the northwestern part of Michigan (lower peninsula).

Jule Crawford
home improvement - Middletown, Connecticut, USA
2004



A. Go to google and type in copper sheet. You will be buried in options. Some building suppliers and some roofing suppliers that are local to you may sell thinner copper. When you say copper, how pure do you want or what alloy do you want. What hardness do you think you need. It all enters into the purchase more than just "copper-at thickness".

James Watts
- Navarre, Florida
2004


Ed. note: Please see letters 17339 and 34185 for some suggested sources, Bruce. Good luck with the project!



(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2025 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"