SPE/SPI STANDARD




I want to know where can I find the SPE/SPI #1, #2 & #3 surface finishing standard ?

Jason S [surname deleted for privacy by Editor]
Mould Making - Singapore
2004



I have been asked about SPI surface finishes, A1 and B3. Is this a specification? If so, where is it available?

Thanks,

Steve S [surname deleted for privacy by Editor]
- Cortland, NY, US
2004



What's the standard of SPI-B3 ?

Pls advise .Thanks.

Allen C [surname deleted for privacy by Editor]
Huiyang city, Guangdong Province, P.R.C.
2004


SPI standards are from the plastics industry and the standard can be found on the Society of Plastics Industry website. www.socplas.org

Chuck Bell
- Buffalo Grove, Illinois, USA
January 28, 2008



letter 20910 explain what the SPI standards are and where to get them, and how we got from the numbered finishes to the lettered finishes. Good luck.

Regards,

Ted Mooney, finishing.com
Ted Mooney, P.E.
Striving to live Aloha
finishing.com - Pine Beach, New Jersey
March 31, 2008




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2025 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"