Theory of electroplating thickness measurement




Where can I get theory behind plating thickness measurement. I desire to calibrate equipment based on kocour method. I am an electronics engineer.

Samvvatsar Sushil
calibration house - Aurangabad, Maharashtra, India
2004


Call the company. They should have some literature available and it will very probably refer to other publications if you want to dig deeper.

James Watts
- Navarre, Florida
2004



DEAR SOHIL

LOOK FOR ISO 2064 IT IS GOOD PLACE FOR YOU TO START.

hadi khosravi
plating and anodizing - tehran iran
2004




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2025 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"