Remove and prevent rust




What chemical can be used to remove rust from the beams of my barns and what can I use to prevent the rusting in the future?

Robert Laird
Farmer - Beaumont, Texas
2004



You can use ammonium citrate solution,5%,pH 3,5- and some epoxy based clearcoat!

Good luck!

Goran Budija
- Cerovski vrh Croatia
2004




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2025 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"