Removing scratches in stainless steel elevator walls




Q. I'm trying to remove scratches in a elevator that has stainless steel walls. Some are not very deep and some are really deep.

Thanks for the help,

Jeff Reinke
Small Business Owner - La Verne, California, USA
2004


A. Deep and light scratches, stains and rust on Stainless steel panels found in elevators are quickly and permanently removed with the Large Area Repair Kit (LARK) by the makers of Scratch-B-Gone; Your First Aid Kit for Stainless steel.

Barry Feinman
Barry Feinman - Chief Restoration Officer
BarrysRestoreItAll
supporting advertiser
Carlsbad, California
barrysrestoreitall
May 2, 2012



Q. I have a very similar problem with several scratches on a brushed steel splashback. I was wondering how you solved the problem.

Dominique Vanthournout
- London, England
2004


Ed. note: See letter 13369. Finishing.com also has a FAQ on "Repairing scratches in stainless steel refrigerator doors" which may be helpful.

none
adv.
this text gets replaced with bannerText
spacer gets replaced with bannerImages



(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2025 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"