Chemical Polish of Jewelry with Thiourea




Hello,

I am a student and I am searching information about a Chemical Process of polish of jewelry with Thiourea this on eBay or Amazon [affil links] (in replace of Cyanide).

Carlos Mauricio Ordoñez
Chemical Engineering Student - Bucaramanga, Santander, Colombia
2004



2003

So what have you learned about it to date, Carlos?

I've seen and heard of cyanide-peroxide "bombing" for chemical polishing (there are several threads on this site about it), and I'd like to hear of a Thiourea this on eBay or Amazon [affil links] alternative myself. Thanks.

Ted Mooney, finishing.com
Ted Mooney, P.E.
Striving to live Aloha
finishing.com - Pine Beach, New Jersey



Carlos,

Thiourea is a mutagen, be careful.

Robert Fyfe
Audio Eng. - Wyoming, NSW, Australia
2004


Hello again.

Ted, right now I don't have any information about the Chemical Polish of gold and silver with Thiourea, so any information that I can get will be very useful for me.

Thanks for your answer.

Carlos Mauricio Ordoñez
- Bucaramanga, Santander, Colombia
2004




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2025 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"