Boring Boron Carbide lame question




Can anyone enlighten me on Boron Carbide finishing? I don't intend to carry it out- I assume its a industrial level job(?) Just out of curiosity I'd appreciate a general outline of the process.

M.Longkumer
Tinkerer - Meghalaya, India
2003



2005

1. You can use a diamond paste lapping if you want to have glaze on a BC body.

2. If you want to coat it, go for plasma/laser/CVD as per your requirement.

Mohanty-Materials Engineer

Rmmohanty
NFTDC - Cuttack




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2024 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"