Info on solar absorber coatings





2003

Dear Sir or Madam,

What is the substance of coated of solar absorber? how can I coat copper sheet?

Best regards,

Persian Energy Policy
Energy Saving - Tehran, Iran



2003

The coating can range from black paint (if the sun is so intense that you don't need to enclose the absorber in glass), through copper oxides and chrome plating, to black chromium plating--and a couple of other coatings as well. You really need to get some books on the subject, which include charts of absorptivity and emissivity and black body radiation coefficients and such things that I haven't taken the time to learn anything about myself :-)

But the most universal coating is probably black chromium plating, which I am told offers very good stability along with good properties for almost any installation.

Ted Mooney, finishing.com
Ted Mooney, P.E.
Striving to live Aloha
finishing.com - Pine Beach, New Jersey




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2025 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"