ted_yosem
Sound technical content, curated with aloha by
Ted Mooney, P.E. RET
Pine Beach, NJ
finishing.com -- The Home Page of the Finishing Industry

  The authoritative public forum
  for Metal Finishing since 1989
  mfhotline


  -----

Silver plating quality problem




We are facing problem of barrel components becomes yellow in dragout of bright silver plating with in 60 sec. This take place only in automatic barrel line.

Please guide.

Shashank
Electrical Eng. Industry - Mumbai, Maharashtra, India
2003



Shashank,

Please tell us if you use potassium cyanide or sodium based silver solution.

Regards,

Anders Sundman
Anders Sundman
4th Generation Surface Engineering
Consultant - Arvika,
Sweden

2003




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2024 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"