Chemical polishing for Stainless Steel




To polish by way of chemical dip or electropolishing for Stainless Steel product in 2B finish stage (301 AISI - nonmagnetic - made of 14% chromium and 2% Nickel )

Rajan
Stainless Steel Utensils Manufacturer - Chennai, Tamilnadu, INDIA
2003



October 2009
"Electroplating Engineering Handbook"
by Larry Durney
EEHcover
on AbeBooks

or eBay or

Amazon

(affil links)

Hi, Rajan. I don't think that a stainless steel with 14% chrome and 2% nickel is type 301 stainless. But the Electroplating Engineering Handbook.
has an excellent chapter about electropolishing of stainless steel. Good luck.

Regards,

Ted Mooney, finishing.com
Ted Mooney, P.E.
Striving to live Aloha
finishing.com - Pine Beach, New Jersey




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2025 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"