Can white gold be electroplated?




Can white gold be electroplated? I want solderable battery contacts. I am considering a gold flash over nickel to make the parts solderable. For cosmetic reasons, I do not want the parts to have a 'gold' color. Is there such a thing as a white gold electroplate?

Mary Davis
- Lynnwood, Washington, USA
2003


Nickel is solderable. Why not matte tin or matte solder over the nickel?

James Watts
- Navarre, Florida
2003



You can use tin plating over your nickel contact. It is both white and solderable.

Neil Bell
Albuquerque, New Mexico
2003



White gold can be electroplated by alloying with other metals. See the Metal Finishing Guide Book & Directory for formulas.

don baudrand
Don Baudrand
Consultant - Poulsbo, Washington
(Don is co-author of "Plating on Plastics" [on Amazon or AbeBooks affil links]
           and "Plating ABS Plastics" [on Amazon or eBay or AbeBooks affil links])
2003




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2025 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"