ted_yosem
Curated with aloha by
Ted Mooney, P.E. RET
finishing.com -- The Home Page of the Finishing Industry

  The authoritative public forum
  for Metal Finishing 1989-2025
  mfhotline


  Thread 21/03

A company that can coat 316ss with black chrome?




Does anyone know of a company that can coat 316ss with black chrome in sheet form?

Clyde Church
- Mason City Iowa
1998
publicly reply to Clyde Church

Black chrome plating on stainess steel is the most popular way of making antennas for vehicles.

I suggest you track down an antenna manufacturer in your part of the world and ask them. It's important to ensure you get a good plater for black chrome, it can suffer from poor quality.

John

John Garvey
wireless technologies - Dublin Ireland
1998
publicly reply to John Garvey


1998

Clyde:

My company colors stainless steel black using a chrome oxide process. We can color 316 grade stainless in sheet. If you have further questions, please feel free to E-Mail me.

Thanks,
Regards,
Bob

Bob Bramson
B&M Finishers / Prismatic Stainless Steel
supporting advertiser
Kenilworth, New Jersey
b&m finishers banner
publicly reply to Bob Bramson



(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2025 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"