PALLADIUM REFINING AND MAKING P-SALT




CAN ANY ONE HELP ME OUT IN MAKING DI NITRO DI AMMINE PALLADIUM SALT (P-SALT) FROM PALLADIUM METAL. AND ALSO PURIFICATION OF PALLADIUM CONTAINING NICKEL , COPPER AND TRACES OF IRON, AS I PLATE OUT THIS FROM DRAGOUTS OF PALLADIUM ON SS CATHODE.

Panjala Mukesh
Panjala Mukesh
fashion jewelry mfgr.
Hyderabad, India

2003



Hi Panjala,

I can't help you but maybe INCO # 2 Research in Port Colborne, Ontario can.

They are or used to extract Pa, Pt and Te from gangue ores and refine them.

You could at least try and ask them. OK?

freeman newton portrait
Freeman Newton [deceased]
(It is our sad duty to advise that Freeman passed away
April 21, 2012. R.I.P. old friend).

2003




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2025 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"