ELECTROPOLISHING TITANIUM




I am seeking anlyte for deburring and electropolishing titanium, preferably without using perchloric and/or hydrofluoric acid.

Joel Levinsohn
Joel Levinsohn
- Sydney, Australia
1998



1998

Hi, Joel:

Long time no hear!

We know of no commercial baths for titanium. The homebrews always contain HF, which is tricky to use.

Regards,
Ed

Ed Bayha
Metal Coating Process Corporation - Charlotte, North Carolina




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2025 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"