How to get FeCl3 from FeCl2





Q. I need some information about the know how of a process of chlorination of a solution of FeCl2 coming from pickling to produce FeCl3.

Alessio Fanciullacci
- Lucca, Tuscany, Italy
2002
publicly reply to Alessio Fanciullacci


A. There is an alternative method: Ferrous Chloride + HCl + O2

adolfo rios pita giurfa
Adolfo Rios Pita Giurfa
- San Isidro, Lima, Peru
2003
publicly reply to Adolfo Rios Pita Giurfa


Q. I need some information about the know how of a process of chlorination of a solution of FeCl2 coming from pickling to produce FeCl3.

Reza Seif Mohaddecy
product designer - Tehran, Iran
April 21, 2008
publicly reply to Reza Seif Mohaddecy

A. Bubble air through it

saeed akbarnejad
- tehran, Iran
May 16, 2010
publicly reply to saeed akbarnejad

A. Yes you can use this equation 2FeCl2 + 2HCl + H2O2 and wait for 3-4 days until the water evaporates and pure FeCl3 is obtained.

Muhammad Danish Ali
Punjab University Lahore - Lahore, Punjab, Pakistan
August 2, 2019
publicly reply to Muhammad Danish Ali



(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2025 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"