Brass Plating




Question, Does anyone know of a non-cyanide brass plating solution? If so, who sells it?

Richard W Howells Jr.
- Erie, Pennsylvania
1998



I believe there are two or three companies which sell non cyanide brass solutions. One which I am aware of is Zinex in California.

Ken Lemke
Ken Lemke
Burlington, Ontario, Canada
1998



As well as Zinex in California , I know that EPI / Electrochemical Products Inc. [a finishing.com supporting advertiser] of New Berlin Wisconsin Sell a Non - Cyanide Brass plating system called E - Brite 44/40 .

John Tenison-Woods
John Tenison - Woods
- Victoria Australia
1998




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2025 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"