Powder coating of wood




I am looking for information on powdercoating wood like what the process is and if I have the correct equipment to do this.

Thank you,

Alan Kirkfield
- Harahan, Louisiana
2002



Alan,

If you are talking about massive wood: forget about it. If you mean MDF: it is possible. If you want general info on the subject: start searching this site using the search engine, look for "MDF". If you want more specific info, tailored for your situation, go to the consultants section of this site.

Best regards,

Remmelt Bosklopper
Remmelt Bosklopper
- Enschede, The Netherlands
2002




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2025 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"