  Thread 155/67

Technical application of Zinc Oxide



Q. I want to use Zinc Oxide in Electroplating. But I want to know that if I buy ordinary commercial grade, what problems I can encounter and also what are the advantages of using a technical grade or elctroplating grade of Zinc Oxide. Can I also know the method and the specifications of the right grade of Zinc Oxide to be used in my application.

Vivek Chandra
- New Delhi, Delhi, India
publicly reply to Vivek Chandra

Zinc Oxide Powder
zinc_powder
on eBay or

Amazon

(affil links)

A. The need for zinc has been answered by commercial zinc ball anodes for decades, may we ask why you want to use zinc oxide instead of zinc ball anodes? What electrolyte do you intend to use? What application do you refer to when you ask us for the "right grade of Zinc Oxide to be used in my application"?

Ted Mooney, finishing.com
Ted Mooney, P.E.
Striving to live Aloha
finishing.com - Pine Beach, New Jersey
publicly reply to Ted Mooney



(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2025 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"