Method to color concrete to near white




Seeking method and or product to color 6000 sq ft of concrete, I do not want to use a top coat of paint, but a dye or stain to use in the mix or after. I am looking to get a lighter than concrete color, not pure white but lighter than the concrete gray.

Thank you,

John Maurer
Freddy's New FRENCHY'S LTD. - Penobsquis, NB, Canada
publicly reply to John Maurer


Stains for Concrete
acid_stain_for_concrete
on eBay or

Amazon

(affil links)

You can get white cement ; aalborg portland white (a Danish product you can buy all over) -use light sand as well - mix it with grey cement and you have a light concrete (can even add diffent other colours).

Karen Marie
- Denmark
publicly reply to Karen Marie



(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2025 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"