Thermal conductive powder





I am looking for information on a thermal conductive powder coating (and company to apply it) that will increase heat dissipation, rather than insulate heat, from outside surface of the aluminum die cast or extruded housing. It very desirable to have nice looking white and/or yellow colors. I am open to suggestions for cost affective alternatives to the powder coating. Heat dissipation, money and color -these are the critical factors.

Boris Shteynberg
- San Francisco, California, USA



Boris,

A silver or white silicone powder will reflect heat from an adjacent source and withstand temperature of 600 F (plus). Automatic application equipment can be provided to precisely control the thickness of powder. If this does not provide the answer, you may want to expand on the requirement.

Herb Ashley
- Smartt, TN



 

Dear Boris,

The Boron Nitride may be suitable for your process needs.
There is a boron nitride coating especially for aluminum die castings; the coating layer will provide the high temperature protection, lubricious surface, anti-corrosive and anti-oxidation.
The boron nitride itself has good thermal conductive of 300 W/mK. It is better them aluminum.

Kent Chu
National Nitride Technologies Co., Ltd. - Taiwan




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2025 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"