What is DIN 50960 plating?



 

I am trying to find information on DIN 50960 plating. What exactly is it (tin/nickel/zinc/etc.)? Is there a website where I can find more info or the full specs?

Thad Rosenberg
- Redwood Falls, MN, USA



Thad -

This standard, as well as most others, can be obtained from Global Engineering.

Cynthia L. Meade
- Sylvania, Ohio, USA



. . . or follow the link to DIN 50960-1. Techstreet offers finishing.com a small commission which covers our time, so we can save you a step by linking directly to the particular spec in question.

I don't believe that DIN 50960 is a particular type of plating, but a document about how to specify plating.

Regards,

Ted Mooney, finishing.com
Ted Mooney, P.E.
Striving to live Aloha
finishing.com - Pine Beach, New Jersey




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2025 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"