Electroless of copper




I want to do electroless cu\ni on glass with a different reducing agent (non formaline).

Maher Shaker Afifi
g.l.s - Cairo



There are e'less Ni baths reduced without formaldehyde, using NaBH4 or DMAB.

James Totter
James Totter, CEF
- Tallahassee, Florida


Dear maher.

I think it is hard to get industrial borane compounds in egypt so I give you my advise to used electroless copper with hypo-phosphite as a reducing agent.

Good luck.

RAAFAT ALBENDARY
plastics electroplating - cairo -egypt




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2025 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"