PEOPLE helping each other -- No AI, cost, registration, or damn popups
(As an Amazon Associate & eBay Partner we earn from qualifying purchases)

Home /
T.O.C.
Fun
FAQs
Good
Books
Ref.
Libr.
Adver-
tise
Help
Wanted
Current
Q&A's
Site 🔍
Search
ted_yosem
Curated with aloha by
Ted Mooney, P.E. RET
finishing.com -- The Home Page of the Finishing Industry

  The authoritative public forum
  for Metal Finishing 1989-2025
  mfhotline


  -----

Chrome Electroplating Aluminum Wheels




1998

Hello,

In New Zealand no-one offers an electroplating service for alloy wheels for cars. I believe this is simply not right and should be fixed. If you know anyone who either does this or supplies a company that does could you forward an address?

Thank you in advance

Dr Stuart Ekdahl (MbChB)
stuartcorp - New Zealand



Macdermid, headquarters in Waterbury Conn., has a very large aluminum wheel plater by the name of PRIME WHEEL, in California.

You can contact MacDermid Australia, or call their U.S. head office.

Ray Delorey
INDUSTRIAL PROCESSING
1997


We have a very modern, fully automatic plating facility in the Philippines. Our capacity is 14000 wheels per month. We plate for Fuzi, Kosei, Enkei, others, and for in house. Technology is a combination of American, German and Japanese, integrated by us, the best of all. Waste treatment is to California standard. Let me know your interest.

Mark Cojuangco
Commplate
1999




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2025 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"