Mg anodizing rack



 

How do you do?

I wondering know that what is using type rack for magnesium anodizing(anomag, algan, magoxid etc..). also, I hope to know suitable material of anodizing rack and what type using when treatment Mg anodizing at your field. I hope to your answer. Thank you.

Kung Su Park
- Korea
publicly reply to Kung Su Park


Magoxid is a patented process, so I would contact the holder of the patent and licensing agent.

tom pullizzi animated    tomPullizziSignature
Tom Pullizzi
Falls Township, Pennsylvania
 
publicly reply to Tom Pullizzi


The Canning Handbook [on eBay, Amazon, AbeBooks affil links] has a little bit on magnesium anodising see page 834.

Martin Trigg-Hogarth
Martin Trigg-Hogarth
surface treatment shop - Stroud, Glos, England
 
publicly reply to Martin Trigg-Hogarth



(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2025 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"