Phosphating system layout & design



Hello dear sir

I research about plant design & layout of phosphating plant.

for example;i want to control phosphating bath or pickling section ,what way can I select for proper design ? what way can I calculate the water or waste water consumption ? the waste water treatment ? IF you help me ? i......

Thanks. king regard

MASOOD RADPEY
SAADAT_ARAK - TEHRAN,TEHRAN,IRAN
2000



Most pretreatment chemical companies can send you a recommended process, depending on your type of parts, production rate, and a whole lot of other variables. You can also contact Chemical Coaters Association International for several manuals dealing with system design and other finishing related topics. You can e-mail me your specifications and I can try to give you some guidance...

Jeff Watson
Jeff Watson
- Pearland, Texas
2000


Dear sir

I am working in car manufacturing company . I have a question about pretreatment line . If we want to use half dip-half spray system(dip-spray)and we have limited area can we use spray system for activation and passivation stages.

with est regards n.mobasseri

mobasseri nasrin
- Tehran,Iran
2001




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread


Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2025 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"